Brand Name : ANSTEEL,TISCO,BAOSTEEL,PANGANGGROUP
Model Number : AISI 660
Certification : SGS,TUV,BV,ISO,MTC
Place of Origin : China
MOQ : Negotiations
Price : Negotiations
Payment Terms : T/T
Supply Ability : 50000KGS/Month
Delivery Time : Ex-stock for delivery: 3-7 days Production lead time: 30-42 days
Packaging Details : Wooden Pallet BOX;Standard Seaworthy Package;based on the customer's special requirement
Product Name : AISI 660 Alloy Steel Plates
Grades : AISI 660
Processing methods : Cold working,Machined
Surface : Bright , Centreless Ground etc.
Profile : Round Bar , Flat Bar , Forging Parts
Price Term : Ex-work
AISI 660 Alloy Steel Plates AISI 660 Superalloy Steel Plates AISI 660 Turbine Blade Steel
Description
Our company provides AISI 660 Alloy Steel Plates AISI 660 Black / Bright / Rrough Turned Turbine Blade Steel AISI 660 Round Bar Peeled / Polished AISI 660 Shot blasted / Ground Flat Bar.
All of AISI 660 Alloy Steel Plates AISI 660 Black / Bright / Rrough Turned Turbine Blade Steel AISI 660 Round Bar Peeled / Polished AISI 660 Shot blasted / Ground Flat Bar conform to Military standard, nuclear power. 100% Ultrasonic test ASTM E2375 /SAE AMS 2154 /SEP 1923 /GB/T 4162 /EN 10228-3.
Products Details
AISI 660 Alloy Steel Plates AISI 660 Black / Bright / Rrough Turned Turbine Blade Steel AISI 660 Round Bar Peeled / Polished AISI 660 Shot blasted / Ground Flat Bar.
Chemical Composition (weight%): | |
C | ≤ 0.08 |
Si | ≤ 1.00 |
Mn | ≤ 2.00 |
P | ≤ 0.040 |
S | ≤ 0.030 |
Cr | 13.5 ~ 16.0 |
Ni | 24.0 ~ 27.0 |
Mo | 1.00 ~ 1.50 |
Ti | 1.90 ~ 2.35 |
Cu | ≤ 0.025 |
Al | ≤ 0.035 |
B | 0.0010 ~ 0.010 |
Mechanical Properties Under Final Heat Treatment: | |
Condition / Bar: Solution treated, precipitation hardened | |
Tensile strength, σb/≥ MPa | 950 |
Yield strength, σ0.2/≥ MPa | 650 |
Elonghation, δ ≥(%) | 12.0 |
Reduction of area, ф ≥ (%) | - |
Hardness | HB | - |
Bars and, where applicable, forgings are subjected to ultrasonic examination based on the different level according to the buyers' requirements.
The alloy is usually produced by AOD / VIM VOD followed by electroslag refining (ESR) or VAR if necessary for special purpose.
FAQ
Q: How do you control the quality?
A: We have professional inspectors to analyze the chemical composition of AISI 660 Alloy Steel Plates AISI 660 Black / Bright / Rrough Turned Turbine Blade Steel AISI 660 Round Bar Peeled / Polished AISI 660 Shot blasted / Ground Flat Bar. and test the finished products in strict accordance with the standards stipulated in the contract. In this process, the inner and outer surfaces, the appearance of both ends, bending, set length, outer diameter and Wall thickness will be checked one by one. You can rest assured that all products you receive from us are reliable.
Q: Do you accept customization?
A: Yes. If you have special requirements for products or packaging, we can make them for you.
Q: Can you accept trial orders?
A: Our MOQ is usually 1 ton. However, if you want to place an order as the start of our cooperation, we can accept smaller quantities at the first time. Of course, after the start, we will have further and longer cooperation.
Q: How do I get samples?
A: Free samples are available for your inspection and testing, DHL/FedEx/UPS accounts can be used for sampling, and the courier fee is borne by you.
Submit an enquiry for the displaying steel materials you are interested in TODAY!
Sales Engineer: sales@ss-bars.com
![]() |
AISI 660 Alloy Steel Plates AISI 660 Superalloy Steel Plates AISI 660 Turbine Blade Steel Images |